A polymer coating of 6:0 mm thickness is cast onto a nonporous flat surface. The coating contains a residual amount of casting solvent, which is uniform at 1.0 wt% within the coating. The mass transfer of solvent through the polymer coating is controlled by molecular diffusion. The air flowing over the coating surface eliminates convective mass-transfer resistances and reduces the solvent vapor concentration in the air to nearly zero. The effective diffusion coefficient of the solvent molecules in the polymer is 2 x 10^-6 cm^2/s.

a. How many hours will it take for the solvent concentration at 1.2 mm from the surface to be reduced to 0.035 wt%?

+5
Answers (1)
  1. 30 October, 15:23
    0
    vent vapor concentration in the air to nearly zero. The effective diffusion coefficient of the solvent molecules in the polymer is 2 x 10^-6 cm^2/s
Know the Answer?
Not Sure About the Answer?
Find an answer to your question ✅ “A polymer coating of 6:0 mm thickness is cast onto a nonporous flat surface. The coating contains a residual amount of casting solvent, ...” in 📘 Chemistry if you're in doubt about the correctness of the answers or there's no answer, then try to use the smart search and find answers to the similar questions.
Search for Other Answers