A cylindrical specimen of a metal alloy 48.0 mm long and 9.72 mm in diameter is stressed in tension. A true stress of 368 MPa causes the specimen to plastically elongate to a length of 53.5 mm. If it is known that the strain-hardening exponent for this alloy is 0.2, calculate the true stress (in MPa) necessary to plastically elongate a specimen of this same material from a length of 48.0 mm to a length of 57.4 mm.
+1
Answers (1)
Know the Answer?
Not Sure About the Answer?
Find an answer to your question ✅ “A cylindrical specimen of a metal alloy 48.0 mm long and 9.72 mm in diameter is stressed in tension. A true stress of 368 MPa causes the ...” in 📘 Engineering if you're in doubt about the correctness of the answers or there's no answer, then try to use the smart search and find answers to the similar questions.